SAI has achieved the production of recycled aluminum with 100% recycled scraps. Through strict quality control and continuous improvement, the cleanliness of SAI’s RESAICAL® recycled aluminum exceeds international standards. The production process reduces waste generation, saves energy, and effectively reduces carbon emissions, which won the recognition of the judges in this competition. At the award ceremony on May 6, Cherng Ming-Shiou, an independent director of SAI, attended the ceremony to receive the award. In his speech, Cherng Ming-Shiou “This is not only the realization of technology, but also a journey of circular economy, helping the automotive industry move towards the goal of low carbon. In the future, SAI will continue to uphold the spirit of sustainable development and continue to move forward on the path of low carbon.”